1 / 6
Model No. : | Titaniun Tube/Pipe |
---|---|
Brand Name : | Torich |
Alloy : | Titanium Pipes |
Ningbo, Zhejiang, China
Описание продукта
Труба сварная бесшовная стальная титановая холоднотянутая ASTM B338 GR2
Химические требования
Composition % | |||||||
Elements | Gr 1 | Gr 2 | Gr 3 | Gr 7 | Gr 9 | Gr 11 | Gr 12 |
N max |
0.03 | 0.03 | 0.05 | 0.03 | 0.03 | 0.03 | 0.03 |
C max | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 |
H max | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 |
Fe Max | 0.20 | 0.30 | 0.30 |
0.30 |
0.25 | 0.20 | 0.30 |
O max | 0.18 | 0.25 | 0.35 | 0.25 | 0.15 | 0.18 | 0.25 |
Al |
|
|
|
|
2.5-3.5 |
|
|
V |
|
|
|
|
2.0-3.0 |
|
|
Pd |
|
|
|
0.12-0.25 |
|
0.12-0.25 |
|
Mo |
|
|
|
|
|
|
0.2-0.4 |
Ni |
|
|
|
|
|
|
0.6-0.9 |
Residuals max each | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 |
Residuals max total | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 |
Ti |
balance |
balance | balance | balance | balance | balance | balance |
Composition % | |||||||
Elements | Gr 13 | Gr 14 | Gr 15 | Gr 16 | Gr 17 | Gr 18 | Gr 26 |
N max |
0.03 | 0.03 | 0.05 | 0.03 | 0.03 | 0.03 | 0.03 |
C max | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 |
H max | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 |
Fe Max | 0.20 | 0.30 | 0.30 |
0.30 |
0.20 | 0.25 | 0.30 |
O max | 0.10 | 0.15 | 0.25 | 0.25 | 0.18 | 0.15 | 0.25 |
Al |
|
|
|
|
|
2.5-3.5 |
|
V |
|
|
|
|
|
2.0-3.0 |
|
Ru |
0.04-0.06 | 0.04-0.06 | 0.04-0.06 |
|
|
|
0.08-0.14 |
Pd |
|
|
|
0.04-0.08 | 0.04-0.08 | 0.04-0.08 |
|
Ni | 0.4-0.6 | 0.4-0.6 | 0.4-0.6 |
|
|
|
|
Residuals max each | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 |
Residuals max total | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 |
Ti |
balance |
balance | balance | balance | balance | balance | balance |
Composition % | ||||||||
Elements | Gr 27 | Gr 28 | Gr 30 | Gr 31 | Gr 33 | Gr 34 | Gr 35 | Gr 36 |
N max |
0.03 | 0.03 | 0.03 | 0.05 | 0.03 | 0.05 | 0.05 | 0.03 |
C max | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 | 0.04 |
H max | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 | 0.0035 |
Fe Max | 0.20 | 0.25 | 0.30 |
0.30 |
0.30 | 0.30 | 0.2-0.8 | 0.03 |
O max | 0.18 | 0.15 | 0.25 | 0.35 | 0.25 | 0.35 | 0.25 | 0.16 |
Al |
|
2.5-3.5 |
|
|
|
|
4.0-5.0 |
|
V |
|
2.0-3.0 |
|
|
|
|
1.1-2.1 |
|
Ru |
0.08-0.14 | 0.08-0.14 |
|
|
0.02-0.04 | 0.02-0.04 |
|
|
Pd |
|
|
0.04-0.08 | 0.04-0.08 | 0.01-0.02 | 0.01-0.02 |
|
|
Co |
|
|
0.20-0.80 | 0.20-0.80 |
|
|
|
|
Mo |
|
|
|
|
|
|
1.5-2.5 |
|
Cr |
|
|
|
|
0.1-0.2 | 0.1-0.2 |
|
|
Ni |
|
|
|
|
|
|
|
42-47 |
Si |
|
|
|
|
|
|
0.20-0.40 |
|
Residuals max each | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 |
Residuals max total | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 |
Ti |
balance |
balance | balance | balance | balance | balance | balance | balance |
Требования к растяжению
Grade |
Tensile strength |
Yield strength | Elongation |
Mpa | Mpa | In 2 in or 50mm min% | |
1 Annealing | 240 | 170-310 | 24 |
2Annealing | 345 | 275-450 | 20 |
3Annealing | 450 | 380-550 | 18 |
7Annealing | 345 | 275-450 | 20 |
9Cold-worked+SR | 860 | 725 min | 10 |
9Annealing | 620 | 483 min | 15 |
11Annealing | 240 | 170-310 | 24 |
12Annealing | 483 | 345 min | 18 |
13Annealing | 275 | 170 min | 24 |
14Annealing | 410 | 275 min | 20 |
15Annealing | 483 | 380 min | 18 |
16Annealing | 345 | 275-450 | 20 |
17Annealing | 240 | 170-310 | 24 |
18Cold-worked+SR | 860 | 725 | 10 |
18Annealing | 620 | 483 | 15 |
26 | 345 | 275-450 | 20 |
27 | 240 | 170-310 | 24 |
28 | 620 | 483 | 15 |
30 | 345 | 275-450 | 20 |
31 | 450 | 380-550 | 18 |
33 | 345 | 275-450 | 20 |
34 | 450 | 380-550 | 18 |
35 | 895 | 828 min | 5 |
36 | 450 | 410-655 | 10 |
Размерный ряд: OD20-28мм WT2,2.5,3мм
OD8 * 1,5 OD12 * 1 OD12,7 * 0,7 OD16 * .08 OD16 * 2 OD 19 * 0,8 OD19 * 1 OD19 / 25 * 2 OD38 * 1 OD50 * 1 OD19 * 1,2 OD25 * 1,2 Также доступны другие размеры.
Применение : Конденсатор и теплообменник авиационного двигателя
Производство м енит: Сварной.
Ningbo, Zhejiang, China
Отправьте запрос этому поставщику